Note 54 bis — Chapter XVIII · SILICON AND THE OTHER ELEMENTS OF THE FOURTH GROUP
George Kamensky translation
Frémy obtained potassium plumbate in the following manner. Pure lead dioxide is placed in a silver crucible, and a strong solution of pure caustic potash is poured over it. The mixture is heated and small quantities are removed from time to time for testing, which consists in dissolving in a small quantity of water and decomposing the resultant solution with nitric acid. There is a certain moment during the heating when a considerable amount of insoluble lead dioxide is precipitated on the addition of the nitric acid; the solution then contains the salt in question, and the heating must be stopped, and a small amount of water added to dissolve the potassium plumbate formed. On cooling the salt separates in somewhat large crystals, which have the same composition as the stannate—that is, PbO(KO)2,3H2O.